Removing Marine Antifouling & Boat Paint from Fibreglass (GRP), Timber & Steel Hulls in New Zealand: The Complete Poultice Stripping Guide

Every winter and spring across New Zealand's premier haul-out yards—from Westhaven, Orams Marine, Half Moon Bay, and Gulf Harbour in Auckland to Tauranga Bridge Marina, Whangārei, Mana, Waikawa, Port Nelson, and Lyttelton—thousands of launch owners, yacht skippers, and commercial shipwrights face the most dreaded job in vessel maintenance: removing ten to twenty seasons of failed, flaking marine antifouling.
Over years of annual haul-outs, rolling fresh ablative or hard cuprous-oxide antifouling over oxidised, leached-out bottom paint creates a thick, brittle, cratered coating stack. Eventually, inter-coat adhesion fails. Large plaques of old antifoul delaminate underway, creating severe hydrodynamic hull drag, driving diesel fuel burn up by 12% to 25%, concealing nascent osmosis blisters in GRP gelcoat, or trapping moisture against historic kauri planking.
Yet traditional removal methods—lying beneath a hull for 40 hours with an orbital sander inhaling toxic copper dust, or paying thousands of dollars for soda or garnet blasting that risks pitting soft gelcoat and violating marina environmental rules—are rapidly becoming obsolete. In this comprehensive 2026 New Zealand marine specification guide, we break down how the patented Peel Away 8 and Peel Away 1 poultice stripping systems remove up to 20+ coats of antifouling and marine enamel in a single dust-free overnight application.
1. The Problem with Multi-Season Antifouling Build-Up in NZ Waters
New Zealand's coastal waters—particularly the warm, nutrient-rich estuaries of the Hauraki Gulf, Bay of Islands, Tauranga Harbour, and Marlborough Sounds—produce some of the most aggressive marine biofouling pressures in the Southern Hemisphere. To combat barnacles, tube worms, bryozoans, and slime, kiwi vessels rely on high-loading cuprous oxide ($\text{Cu}_2\text{O}$), copper thiocyanate, and organic co-biocide antifouling formulations.
Why Layering New Antifoul Over Old Eventually Fails
Even self-polishing copolymer (SPC) and ablative antifoulings do not wear away uniformly. High-flow zones along the bow forefoot, keel leading edge, and rudder polish thin, while lower-turbulence zones under the bilge turn, transom, and shaft struts accumulate 1.5mm to 4.0mm of spent resin skeleton. After 5 to 15 haul-out cycles, three critical failure mechanisms emerge:
- Hydrodynamic Drag & Fuel Penalty: Once an aged antifouling stack begins to "alligator" (micro-crack) and flake, surface roughness jumps from a smooth 30–50 microns to over 500–1,200 microns. Naval architecture studies demonstrate that a rough, cratered antifouling film increases skin-friction resistance enough to reduce cruising speed by 1.5 to 3 knots and increase diesel consumption on planing and displacement launches by 12% to 25%.
- Leached-Out Biocide Skeletons & Inter-Coat Delamination: In hard modified-epoxy and rosin-based antifoulings, once the soluble copper biocide leaches out, a porous, brittle honeycombed resin matrix remains. Applying fresh solvent-rich antifoul over this oxidized skeleton causes solvent shock and shrinkage tension, shearing the old layers right off the primer as soon as the vessel hits 15 knots.
- Concealed Osmosis & Timber Fastening Decay: On GRP fibreglass hulls built prior to iso/vinylester barrier adoption, thick paint build-up hides acidic glycol osmosis blisters festering beneath the gelcoat. On traditional New Zealand carvel, clinker, or diagonal double-skin kauri and totara hulls, heavy paint accumulation bridges plank seams, traps bilge and hull moisture, and masks electrolytically corroded bronze or copper fastenings.
2. Why Dry Sanding, Soda Blasting & Aggressive Solvents Threaten Hulls and Boatyards
When a hull reaches the point where it must be taken back to bare gelcoat, epoxy primer, timber, or steel, vessel owners and boatyard managers must weigh substrate preservation against strict New Zealand environmental regulations.
1. Mechanical Orbital Sanding & Carbide Scraping
Grinding overhead with 40-to-80 grit discs on a random orbital sander—even when connected to an industrial shop vacuum—is punishing, slow, and hazardous:
- Gelcoat Thinning & Profiling Damage: Factory polyester gelcoat below the waterline is typically only 0.4mm to 0.6mm (400–600 microns) thick. Aggressive rotary sanding inevitably gouges chine edges, strakes, and keel fillets, thinning the moisture barrier and accelerating osmotic water ingress into the chopped-strand mat laminate.
- Scorching Kauri & Cedar Planking: On classic New Zealand timber launches and yachts, heavy sanding dishes out softer earlywood grain between fasteners, destroys fair hull lines, and exposes cotton caulking or spline gluelines.
- Toxic Biocide Dust Exposure: Antifouling dust contains 30% to 60% cuprous oxide, zinc oxide, zineb, and—on older vessels laid up decades ago—legacy organotin compounds such as tributyltin (TBT) or lead-based primers. Without full positive-pressure air-fed respirators and sealed tenting, sanding dust poses severe acute respiratory and neurotoxic hazards.
2. Abrasive Blasting (Soda, Garnet, Crushed Glass & Slurry Blasting)
While mobile slurry or soda blasters can strip a 40ft hull in a day, the hidden costs and substrate risks are substantial:
- Micro-Pitting Requiring Complete Hull Refairing: Even "gentle" sodium bicarbonate (soda) or fine garnet media relies on high-velocity kinetic impact. On GRP hulls, blasting frequently opens pinholes and micro-voids across the gelcoat surface, forcing the owner to spend thousands of dollars trowel-fairing the entire underwater hull with two-pack epoxy fairing compound before barrier coats can be rolled.
- Marina Hardstand Bans & Expensive Tenting: Most premier New Zealand marinas—including Westhaven Marina, Half Moon Bay Marina, Gulf Harbour Marina, Tauranga Bridge Marina, Waikawa Marina, and Port Nelson—strictly prohibit open-air abrasive blasting on standard hardstand bays. Hiring a shrink-wrapped environmental containment tent, mobile blast rig, and spent-media hazardous waste disposal routinely pushes the bill for a 40ft vessel past $4,500–$7,500+ NZD.
3. Conventional Solvent Paint Strippers
Hardware-store liquid solvent strippers containing dichloromethane (methylene chloride), ketones, or aromatic hydrocarbons must never be used on fibreglass (GRP) or composite vessels. Aggressive organic solvents attack the ester and styrene linkages in cured polyester and vinylester gelcoats, permanently softening, blistering, and crazing the structural skin of the boat.
3. Table 1 — Technical Comparison Matrix: Marine Hull Stripping Systems in New Zealand
The engineering comparison matrix below evaluates the four primary methods for stripping underwater antifouling and topside marine paints across New Zealand hardstands:
| Performance & Compliance Parameter | Peel Away 8 (pH-Neutral Marine Poultice — GRP & Alloy) | Peel Away 1 (Alkaline Poultice — Timber & Steel Hulls) | Abrasive / Soda / Garnet Blasting | Mechanical Orbital / Scraper Sanding |
|---|---|---|---|---|
| GRP Gelcoat & Composite Safety | 100% Safe — Solvent-free, pH-neutral; zero styrene attack, softening, or micro-pitting | Not recommended for bare GRP gelcoat or aluminium (use Peel Away 8 instead) | High Risk — Pits gelcoat and exposes laminate pinholes requiring full epoxy fairing | Moderate-High Risk — Thins gelcoat on chines/keel and leaves deep swirl scratches |
| Airborne Copper & Biocide Dust Containment | 100% Dust-Free — Wet paste + laminated blanket traps all Cu₂O and biocides in solid state | 100% Dust-Free — Fully encapsulates red-lead primers, TBT, and copper antifoul | Severe plume unless full negative-pressure shrink-wrap tenting is erected | High airborne toxic dust even with vacuum-shrouded sanders |
| Single-Pass Coat Removal Capacity | 10 to 20+ coats of ablative, hard, or copolymer antifouling in one overnight pass | Up to 30 coats of aged alkyd enamel, red lead, coal-tar epoxy, and antifouling | Single pass, but struggles with elastic high-build membranes | Clogs discs rapidly on soft ablative antifoul; requires 30–60+ labour hours |
| NZ Marina Hardstand Compliance | Approved on open hardstand bays with drop-sheet & sump wash-down interceptor | Approved on hardstands with standard drop-sheet containment & neutralisation | Prohibited on open hardstand bays at most NZ marinas without full encapsulation | Strictly policed; dry sanding without 100% vacuum capture is banned |
| Typical Material / Contractor Cost per m² (NZD) | $48 – $62 / m² (DIY/Yard Material Cost incl. Peel Away Paper) | $52 – $68 / m² (DIY/Yard Material Cost incl. Paper & Neutraliser) | $135 – $240+ / m² (plus tenting, haul-out relocation & epoxy refairing) | $30 – $45 / m² in abrasive discs + $95 – $160 / m² in yard labour |
4. Selecting the Right System by Hull Substrate: GRP, Aluminium, Timber & Steel
Matching the correct Peel Away formulation to your vessel's hull material and coating history ensures rapid stripping without chemical incompatibility:
1. GRP Fibreglass / Gelcoat, Carbon Composite & Marine Aluminium Hulls — Mandatory Peel Away 8
For 95% of modern recreational trailer boats, production cruisers, racing keelboats, and catamarans in New Zealand, Peel Away 8 is the mandatory specification:
- Zero Alkaline Saponification of Polyester/Vinylester Gelcoat: Standard polyester gelcoat is an ester-based polymer. Strong caustic alkalis (sodium or potassium hydroxide) can saponify ester linkages over prolonged exposure. Because Peel Away 8 is pH-neutral, non-caustic, and biodegradable, it cleaves the rosin, acrylic, or copolymer binders in marine antifouling while leaving polyester, vinylester, and epoxy gelcoats completely untouched.
- Safe for 5083 / 5086 Marine-Grade Aluminium Hulls & Outdrives: Strong caustic strippers react amphotericly with bare aluminium alloy, etching plate surfaces and evolving hydrogen gas. Peel Away 8's pH-neutral formulation safely removes Trilux, copper-free thiocyanate antifoulings, and polyurethane topside enamels from alloy trailer boats, commercial catamarans, and Saildrive legs without corroding the metal.
- Preserves or Removes Epoxy Barrier Coats by Dwell Control: Because Peel Away 8 acts progressively from the outer layer inward, shipwrights can calibrate dwell time (typically 8–14 hours) to strip 10+ layers of ablative antifoul while preserving a sound 2-pack epoxy barrier coat beneath—or leave it sealed for 24–36 hours to strip failed single-pack primers all the way to bare gelcoat.
2. Traditional NZ Kauri/Totara Timber Hulls & Steel Vessels — Peel Away 1 or Peel Away 8
New Zealand boasts one of the world's finest fleets of classic Logan, Bailey, Lidgard, and Mullet boats built from heart kauri, alongside heavy displacement steel cruising yachts and commercial fishing vessels:
- Classic Timber Hulls (Carvel, Clinker & Double-Diagonal Kauri): Centuries-old or mid-century timber vessels frequently carry 15 to 30 coats of traditional linseed-oil lead primers, red lead below the waterline, alkyd marine enamels, and hard copper antifouling. Peel Away 1 saponifies these heavy oil and lead stacks in a single application without gouging soft kauri planking or disturbing cotton seam caulking. After washing down, timber hulls stripped with Peel Away 1 must be treated with Peel Away Neutraliser to restore timber pH to 6.5–7.5 before applying new marine primers.
- Steel Yachts & Commercial Vessels (Proven on the Mayling Yacht Restoration at Port Nelson): Both Peel Away 8 and Peel Away 1 perform exceptionally on steel hulls. In our landmark Mayling Yacht project at Port Nelson—executed by MarineWorx NZ Ltd—Peel Away 8 was selected to strip multiple layers of aged marine coatings from the steel yacht's hull on the hardstand with full environmental encapsulation, zero fumes, and zero dust. For industrial steel structures with 20–30 coats of legacy red-lead primer—such as the Auckland Harbour Bridge lead abatement—Peel Away 1 delivers unmatched single-pass stripping power (and steel surfaces do not require acid neutralisation after Peel Away 1).
5. 8-Step NZ Hardstand & Boatyard Application Specification
To achieve a clean, single-pass antifouling strip during a standard weekend or mid-week marina haul-out, follow this 8-step boatyard specification (also cross-referenced on our Application Guides hub):
Step 1: High-Pressure Lift-Out Wash & Waterline Masking
Immediately upon haul-out in the travel-lift sling, have the yard operator pressure-wash marine slime, weed, and loose barnacles from the hull while it is still wet. Once chocked on the hardstand and dry, lay a heavy-duty 200-micron polythene drop-sheet beneath the keel and bilge props to catch any paste drips. Mask the boot-top waterline, depth-sounder transducers, bronze skin fittings, and sacrificial zinc anodes using high-tack Cloth Duct Tape.
Step 2: Mandatory 24-Hour Trial Patch Dwell Calibration
Every boat's underwater paint history is unique—often mixing incompatible hard racing copper paints over soft ablative layers. Before applying paste to the whole hull, apply a 300mm x 300mm test patch of Peel Away 8 (or Peel Away 1 on heavily layered timber/steel) at 2.5mm–3.5mm thickness near the waterline and bilge turn. Check at 8, 12, and 24 hours to verify the exact dwell window that strips all antifoul layers cleanly down to the barrier coat or gelcoat.
Step 3: 2mm–4mm Trowel, Roller, or Airless Spray Application
Apply Peel Away paste evenly across the underwater hull at a thickness of 2.0mm to 3.5mm (or up to 4.5mm on heavy 15+ season keel and rudder build-ups):
- DIY & Owner-Operators: Apply quickly using a 200mm flexible stainless-steel or plastic broad-knife, plasterer's trowel, or long-nap texture roller, followed by smoothing with the supplied Peel Away spatula.
- Commercial Shipwrights & Boatyards: On 40ft–70ft launches and commercial vessels, pump Peel Away 8 through a heavy-duty Graco or Wagner airless texture sprayer (minimum 1:30 pump ratio, hoses with filters removed, 0.029" to 0.035" reversible tip), coating an entire 45ft hull in under two hours.
Step 4: Laminated Blanket Sealing Against Coastal Wind Drying
New Zealand marina hardstands are notoriously windy. Immediately cover the wet paste with genuine printed Peel Away Laminated Paper (printed logo side facing outward). Smooth the blanket onto the hull using a soft brush or plastic smoother from the centre outward to expel trapped air pockets. Overlap adjacent sheets by 25mm and seal all lower keel edges and waterline margins with Cloth Duct Tape so sea breezes cannot dry the poultice prematurely.
Step 5: 12–24 Hour Overnight Dwell
Leave the encapsulated hull to dwell overnight (typically 12 to 24 hours for Peel Away 8 on 5–15 coats of antifouling in 12°C–22°C ambient temperatures, or up to 36–48 hours in cold South Island winter haul-outs). Inside the vapour-tight laminated blanket, the poultice paste penetrates every coat, breaking the resin bond at the gelcoat or barrier-coat interface.
Step 6: Solid Poultice Peel-Off into Lined Drums
Working in 1 m² to 2 m² sections, slide a rounded-corner broad plastic or stainless-steel scraper behind the laminated cover sheet at a shallow 30-degree angle. Peel the blanket away from the hull: 85% to 95% of the softened antifouling stack lifts off in a solid, damp ribbon bonded directly to the paper. Fold each stripped sheet inward upon itself and deposit it directly into heavy-duty 200-micron hazardous waste bags or poly-lined 200L marina waste drums.
Step 7: Low-Pressure Hardstand Wash-Down Over Sump Interceptor Traps
Before the thin residual film on the hull can dry, scrub the section with a stiff nylon deck brush and wash down using a low-pressure fresh-water hose or fan-tip pressure washer (500–1,000 PSI max). Roll up the ground polythene drop-sheet containing any solid paste flakes, allowing only the fine rinse water to flow into the marina hardstand's trade-waste collection sump and heavy-metal interceptor trap.
Step 8: pH & Moisture Verification Before Epoxy Barrier Coating
- After Peel Away 8 (GRP, Composite, Alloy, Steel): Because Peel Away 8 is pH-neutral, zero chemical neutralisation is required. Allow the hull to dry for 24–48 hours, give the clean gelcoat or intact epoxy primer a light pass with 80-to-120 grit paper to establish a mechanical key, solvent-wipe, and apply your two-pack epoxy barrier coat or new antifouling system.
- After Peel Away 1 (Timber & Steel Hulls): On kauri or timber hulls, spray on Peel Away Neutraliser, brush into plank seams, rinse with fresh water, and verify a neutral pH of 6.5–7.5 and timber moisture content below 12%–14% before priming.
6. NZ Regional Council & Marina Hardstand Environmental Compliance
Environmental enforcement across New Zealand boatyards has tightened dramatically under the Resource Management Act 1991 (RMA Section 15 — Discharge of Contaminants into Water or onto Land), the Auckland Unitary Plan Coastal & Stormwater provisions, and the New Zealand Clean Marina Program.
- Zero Uncontained Biocide Discharge: Discharging copper-laden sanding dust or untreated paint-stripping sludge into coastal marine areas or municipal stormwater networks carries severe infringement fines from Auckland Council, Bay of Plenty Regional Council, Greater Wellington, Nelson City Council, and Environment Canterbury. Because Peel Away captures over 90% of the copper, zinc, and lead paint mass inside the solid laminated paper blanket prior to washing, solid toxic waste is completely diverted from the wash-water stream.
- Compatibility with Marina Wash-Water Filtration Plants: Modern NZ hardstands circulate wash-down runoff through three-stage grit interceptors, hydro-cyclones, and activated-carbon/ion-exchange media beds to strip dissolved copper before discharging to trade waste. Unlike solvent strippers that emulsify oils and foul marina carbon filters, Peel Away 8 is water-based and solvent-free, ensuring full compatibility with boatyard treatment plants.
- WorkSafe NZ Respiratory & PPE Controls: Under the Health and Safety at Work Act 2015 (HSWA), boatyard employers and contractors must eliminate or minimise exposure to hazardous substances. By replacing dry orbital sanding with wet poultice stripping, airborne copper and silica dust is eliminated at the source. Always wear chemical-resistant nitrile gloves, wrap-around safety goggles, coveralls, and enclosed boots, and review our downloadable SDS and SWMS documents on our Safety & Compliance page.
7. Table 2 — 2026 NZ Vessel Hull Surface Area, Pail Coverage & Cost Estimator
To calculate how much Peel Away 8 (or Peel Away 1) your vessel requires, you can estimate underwater wetted hull surface area ($\text{WSA}$) using the standard naval formula $\text{WSA} \approx \text{LWL} \times (\text{Beam} + \text{Draft}) \times 0.75$ for power launches or $\times 0.65$ for fin-keel yachts. At a 2.5mm–3.5mm marine application thickness, one 15kg trade pail ($360.00 NZD excl. GST) covers 6.5 to 8.0 m²:
| Vessel Class & Length Overall (LOA) | Typical Wetted Hull Area (m²) | 15kg Peel Away 8 / PA-1 Pails Required | Laminated Paper & Tape Pack Allocation | Total Material Cost (NZD Excl. GST)* |
|---|---|---|---|---|
| 24ft Trailer Launch / Keeler (7.3m) | ~16 m² | 2 x 15kg Trade Pails (30 kg) | Included sheets + 1 x 10-Pack Paper ($27.50) & 2 x Cloth Tape ($14.00) | $761.50 NZD (~$47.60 / m²) |
| 32ft–36ft Cruiser / Launch / Yacht (10m–11m) | ~28 m² | 4 x 15kg Trade Pails (60 kg) | Included sheets + 1 x 20-Pack Paper ($55.00) & 3 x Cloth Tape ($21.00) | $1,516.00 NZD (~$54.15 / m²) |
| 42ft–45ft Flybridge Launch / Keelboat (13m–14m) | ~44 m² | 6 x 15kg Trade Pails (90 kg) | Included sheets + 2 x 20-Pack Paper ($110.00) & 4 x Cloth Tape ($28.00) | $2,298.00 NZD (~$52.20 / m²) |
| 55ft–65ft Commercial / Charter Vessel (17m–20m) | ~75 m² | 10 x 15kg Trade Pails (150 kg) | Included sheets + 3 x 20-Pack Paper ($165.00) & 6 x Cloth Tape ($42.00) | $3,807.00 NZD (~$50.75 / m²) |
*Note: 2026 New Zealand trade material pricing based on $360.00 excl. GST per 15kg pail of Peel Away 8 or Peel Away 1 (each 15kg pail includes laminated cover sheets; additional Peel Away Paper packs are recommended for complex hull curvature). If using Peel Away 1 on a timber hull, add 1 x 5kg ($130.00) or 15kg ($350.00) Peel Away Neutraliser. Order direct via our Online Shop or Request a Trade Boatyard Quote.
8. Frequently Asked Questions: Marine Antifouling & Boat Paint Removal in NZ
1. Will Peel Away 8 damage fibreglass (GRP) gelcoat or trigger osmosis blistering?
No. Peel Away 8 is a solvent-free, non-caustic, pH-neutral poultice paste specifically formulated for safe use on polyester, vinylester, and epoxy GRP gelcoats. Unlike aggressive methylene chloride or ketone solvents that attack styrene cross-links, or caustic alkaline strippers that cause ester saponification in polyester gelcoat, Peel Away 8 breaks down the antifouling resin matrix without softening, etching, or thinning the underlying gelcoat or two-pack epoxy barrier coat.
2. How many coats of marine antifouling can Peel Away 8 remove in a single application?
When applied at a 2.5mm to 4.0mm thickness and sealed beneath genuine Peel Away laminated cover sheets for 12 to 24 hours, Peel Away 8 routinely strips 10 to 20+ seasonal layers of ablative, copolymer, and hard cuprous oxide antifouling in a single pass—saving 70% to 85% of the manual labour required for wet orbital sanding or hand scraping.
3. When should I use Peel Away 1 vs. Peel Away 8 on a boat hull?
Use Peel Away 8 on all GRP fibreglass/gelcoat hulls, carbon composite hulls, and marine-grade aluminium (5083/5086) vessels, as well as on timber or steel hulls where a pH-neutral, non-neutralising strip is preferred (as proven on the Mayling Yacht Restoration at Port Nelson). Use Peel Away 1 (alkaline poultice) on traditional New Zealand kauri, totara, or cedar planked timber hulls and heavy commercial steel vessels coated with up to 30 layers of legacy oil-based marine enamels, red-lead primers, and hard antifouling. Timber hulls stripped with Peel Away 1 must be treated with Peel Away Neutraliser prior to fairing and epoxy priming; steel hulls do not require neutralisation.
4. Is Peel Away compliant with New Zealand marina hardstand and Regional Council environmental rules?
Yes. Major New Zealand marinas—including Westhaven, Half Moon Bay, Gulf Harbour, Orams Marine, Tauranga Bridge Marina, Waikawa, and Port Nelson—prohibit dry sanding and uncontained open-air grit or soda blasting because airborne copper, zinc pyrithione, and legacy tributyltin (TBT) biocides contaminate harbour waters. Peel Away encapsulates 90%+ of the dissolved antifouling inside the solid paste and laminated blanket for direct drum disposal, while final low-pressure rinse water passes cleanly through standard marina hardstand sump interceptor traps under RMA Section 15 trade-waste rules.
5. Can Peel Away 8 strip antifouling without removing an intact two-pack epoxy barrier coat underneath?
Yes, by calibrating dwell time via a trial patch. High-solids cured two-pack marine epoxy barrier coats (such as Interprotect or West System) have significantly higher cross-link density than single-pack ablative or hard acrylic/rosin antifouling. A 8-to-14 hour dwell time with Peel Away 8 will typically release the multi-season antifouling stack while leaving a sound, well-cured epoxy barrier coat intact. If you want to strip the epoxy barrier coat as well down to bare gelcoat for osmosis repair, extend the dwell time to 24–36 hours.
6. How many 15kg pails of Peel Away 8 do I need for a 35ft or 45ft launch or yacht?
At a standard 2.5mm–3.5mm marine application thickness, one 15kg trade pail of Peel Away 8 covers approximately 6.5 to 8.0 m² of underwater hull area. A typical 32ft–36ft launch or cruising yacht (~28 m² wetted surface area) requires four 15kg pails ($1,440 NZD excl. GST), while a 42ft–45ft flybridge launch or keelboat (~44 m² wetted hull area) requires six 15kg pails ($2,160 NZD excl. GST).
7. How long must a timber or fibreglass hull dry after Peel Away stripping before applying epoxy barrier coats?
After peeling off the laminated cover sheets and completing the low-pressure fresh-water wash-down (and Peel Away Neutraliser rinse if Peel Away 1 was used on timber), allow a GRP fibreglass hull 24 to 48 hours in dry conditions to reach surface equilibrium before final 80-grit keying and epoxy barrier coating. On traditional carvel or cold-moulded kauri timber hulls, allow 3 to 7 days until a pin-type or dielectric marine moisture meter confirms timber moisture content is below 12%–14% and surface pH is between 6.5 and 7.5.
Order Marine Trial Kits or Trade Pails for Your Next Haul-Out
Don't waste your limited hardstand haul-out window choking on toxic copper sanding dust or paying thousands for destructive hull blasting. Whether you are stripping a 24ft trailer boat in your driveway, refitting a classic kauri launch at Westhaven, or managing a commercial vessel haul-out at Port Nelson or Tauranga, Peel Away New Zealand ships nationwide within 1–4 business days.
📞 Call John Downey & our marine technical team: 0800 787 472 or 021 950 699
📩 Email for boatyard specifications & trial patch advice: john@peelaway.co.nz
🛒 Order 350g Trial Pots, 5kg Kits, or 15kg Trade Pails online: Shop Peel Away NZ or Request a Bulk Boatyard Quote
Share this article
Related Articles

July 1, 2025
The Safer, Smarter Way to Remove Paint in New Zealand: Why More Professionals Are Choosing Peel Away

June 15, 2025
How to Remove Lead and Asbestos Paint Safely in New Zealand: A Modern Approach for Old Problems

June 1, 2025